Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PAPERMATCH® H-3818 Specialty Masterbatch

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PAPERMATCH® H-3818 Specialty Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPAPERMATCH® H-3818 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® H-3818 is a natural color, low opacity grade designed to provide maximum film stiffness when used in the core, or skin layers, of a coextruded structure. PAPERMATCH® H-3818 is typically recommended for use at 40 to 60% depending upon customer specific application requirements. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 40 %
40 %
ASTM D2765
Descriptive Properties Value Comments
Moisture 1000
ppm, ASTM D789 @ 190°C
Pellet Count 60
pellets/gram
Copyright © lookpolymers.com All Rights Reserved