A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PAPERMATCH® T-4228-8 Specialty Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to provide a smooth surface finish. PAPERMATCH® T-4228-8 is generally recommended for cast or blown film applications at 50% usage levels in HDPE.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.69 g/cc
1.69 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 66 %
66 %
ASTM D2765
Descriptive Properties Value Comments
Moisture 800
ppm, ASTM D789 @ 190°C
Pellet Count 30
pellets/gram