A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® FSU-105 is a general-purpose oleamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF values have been optimized to these addition ratios. POLYBATCH® FSU-105 can typically be used at 1 to 3% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Loss On Ignition 10 %
10 %
ASTM D2584
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 190 °C
23 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Descriptive Properties Value Comments
Adhesive Content 0.05
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 70
pellets/gram