A. Schulman POLYBATCH™ Green P30244/4 Concentrate Based In Copolymer PP

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Green P30244/4 Concentrate Based In Copolymer PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® P30244/4 is a green color concentrate based in Copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically recommended for use at 4% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 2.2 %
2.2 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 55
pellets/gram