A. Schulman POLYBATCH™ Redwood 10416U Concentrate Based In LLDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Redwood 10416U Concentrate Based In LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® 10416U is a redwood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability in polyolefin plastic lumber or injection molding applications. POLYBATCH® 10416U is heavy metal free and is typically recommended for use at 2% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.89 g/cc
1.89 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 64 %
64 %
Descriptive Properties Value Comments
Moisture (max) 2000
ppm, ASTM D789
Pellet Count 35
pellets/gram