Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYBATCH™ U-7025-CFK Blowing Agent Concentrate Based In Polystyrene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ U-7025-CFK Blowing Agent Concentrate Based In Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® U-7025-CFK is a non-tinting, endothermic blowing agent concentrate based in polystyrene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Additive Loading 25 %
25 %
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 45
pellets/gram