Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYBATCH™ UVK-90 UV Stabilizer Concentrate Based In Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ UVK-90 UV Stabilizer Concentrate Based In Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® UVK-90 is a UV stabilizer concentrate containing 10% hindered amine light stabilizer based in polyethylene. This concentrate is designed for use in LDPE, LLDPE, and HDPE applications where high clarity is not required. POLYBATCH® UVK-90 is typically used at 2 to 8% addition levels depending upon application requirements. ApplicationPOLYBATCH® UVK-90 can be used in film, sheet extrusion, and injection molding applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Additive Loading 10 %
10 %
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 40 %
40 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 70
pellets/gram