A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phenolic yellowing/pinking, while optimizing whiteness and thermal stability. POLYBATCH® LL8425 AP also provides optimal dispersion and opacity with excellent letdown mixing. POLYBATCH® LL8425 AP is recommended for use in extrusion film and sheet as well as injection molding applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.93 g/cc
1.93 g/cc
ASTM D792
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 70 %
70 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 30
pellets/gram