Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYBATCH™ White P8550 C Concentrate Based In Polypropylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ White P8550 C Concentrate Based In Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® P8550 C is a white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product is stearate free and has been designed to offer good dispersion and excellent letdown mixing in injection, and blow molding applications. POLYBATCH® P8550 C is typically recommended for use at 2 to 4% addition levels depending upon application requirements. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1500
ppm, ASTM D789
Pellet Count 25
pellets/gram