A. Schulman POLYBLAK™ 2076 Superior Black Color Concentrate, 40% Carbon Black Based In EVA

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 2076 Superior Black Color Concentrate, 40% Carbon Black Based In EVA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBLAK® Black 2076 is a superior black color concentrate containing 40% carbon black in EVA. This masterbatch is designed to provide good opacity and a regular blue undertone with pigment particle size of 70 nanometers. POLYBLAK® Black 2076 is formulated for use in injection molding applications. POLYBLAK® Black 2076 is typically recommended for use at 5% addition levels.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Carbon Black Loading 40 %
40 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789