A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Index of Compound 4.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.86 J/cm
9.10 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 159 °C
318 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 111 °C
232 °F
ASTM D648