Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Melt Flow 4.0 - 8.0 g/10 min
4.0 - 8.0 g/10 min
ASTM D1238
Users viewing this material also viewed the following: