Material Notes:
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
UL RTI, Electrical 105 °C
221 °F
0.030 in; UL 94
Flammability, UL94 V-2

@Thickness 0.780 mm
V-2

@Thickness 0.0307 in
V-2

@Thickness 1.57 mm
V-2

@Thickness 0.0618 in
V-2

@Thickness 3.05 mm
V-2

@Thickness 0.120 in