Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Melt Flow 20 - 30 g/10 min

@Temperature 230 °C
20 - 30 g/10 min

@Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 29.7 MPa
4310 psi
ASTM D638
Flexural Modulus 3.585 GPa
520.0 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.68 J/cm
5.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ASTM D648