A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplications of FPP 1068-32 include electrical connections, ducts, impeller and housings. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 0.220 J/cm
0.412 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ASTM D648