Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 5.0 - 10 g/10 min

@Temperature 230 °C
5.0 - 10 g/10 min

@Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved