A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648