Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.25 g/cc
1.20 - 1.25 g/cc
ASTM D792
Melt Flow 7.0 - 10 g/10 min

@Temperature 230 °C
7.0 - 10 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R >= 80
>= 80
ASTM D785
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
Elongation at Break >= 6.0 %
>= 6.0 %
ASTM D638
Flexural Modulus >= 3.40 GPa
>= 493 ksi
ASTM D790
Izod Impact, Notched >= 0.294 J/cm
>= 0.550 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 120 °C
>= 248 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) >= 90.0 °C
>= 194 °F
ASTM D648
Users viewing this material also viewed the following: