A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648