Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 19 g/10 min
19 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648