A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 3459 is a 30% glass filled copolymerInformation provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Modulus 4.075 GPa
591.0 ksi
ASTM D790
Izod Impact, Notched 2.59 J/cm
4.85 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ASTM D648