A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FXP 2779U is a 20% talc-filled, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.710 J/cm
1.33 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D648