A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Polypropylene (PP)
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Izod Impact, Notched 0.650 J/cm
1.22 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ASTM D648