Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.903 g/cc
0.903 g/cc
ASTM D792
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Falling Dart Impact 10.8 J
8.00 ft-lb
ASTM D3209
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648