A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible to those that are used by Eastman.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.903 g/cc
0.903 g/cc
ASTM D792
Melt Flow 8.0 - 15 g/10 min
8.0 - 15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.8 MPa
5190 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.653 GPa
239.8 ksi
ASTM D790
Izod Impact, Notched >= 0.267 J/cm
>= 0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 101 °C
>= 214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) >= 60.0 °C
>= 140 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Users viewing this material also viewed the following: