A. Schulman POLYFORT™ PX 1040

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PX 1040.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.00 MPa
870 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 4.00 MPa
580 psi
ASTM D790
Flexural Modulus 0.0950 GPa
13.8 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256