Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized by the addition of concentrates.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ASTM D2240
Tensile Strength, Yield 28.1 MPa
4070 psi
ASTM D638
Elongation at Break 480 %
480 %
ASTM D638
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
0.550 J/cm

@Temperature -30.0 °C
1.03 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648