A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion in combination with good impact strength. ApplicationTypical applications include automotive claddings and radiator grills. TPP 530 is paintable with conventional TPO paint systems. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
as molded
0.0090 cm/cm
0.0090 in/in
± 0.1 after 30 min. at 120°C
Melt Index of Compound 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 20.0 °C
28.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Brittleness Temperature -15.0 °C
5.00 °F
Users viewing this material also viewed the following: