A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman.
Physical Properties Metric English Comments
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 10 %
10 %
at max load; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
at 0°F; ASTM D256
0.641 J/cm
1.20 ft-lb/in
ASTM D256
Gardner Impact >= 10.2 J
>= 7.50 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Users viewing this material also viewed the following: