Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 2.0 - 4.0 g/10 min
2.0 - 4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
Izod Impact, Notched 5.30 J/cm
9.93 ft-lb/in
ASTM D256
Gardner Impact 17.0 J

@Temperature -30.0 °C
12.5 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648