Material Notes:
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength at Break 20.7 MPa
3000 psi
at max load; ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Gardner Impact 33.9 J
25.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648