A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical applications of PP 1248-01 are packaging articles and thin-walled containers. This resin meets FDA Regulation 21 CFR 177.1520, for all packaging applications, at temperatures not exceeding 212°F (100°C).Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 32.0 MPa
4640 psi
at 50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
50 mm span, 5 mm/min, tangent; ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648