A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 16 - 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 - 24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Gardner Impact 5.88 J

@Temperature -28.9 °C
4.34 ft-lb

@Temperature -20.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.9 °C
183 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ASTM D648