Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520 and UL 94 HB rating. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
5 mm/min, tangent; ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
ASTM D648