Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
6.78 J

@Temperature -29.0 °C
5.00 ft-lb

@Temperature -20.2 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648