Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 1.5 g/10 min

@Temperature 230 °C
1.5 g/10 min

@Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Users viewing this material also viewed the following: