Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer A. Schulman, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, rope and twine. PP 3468-01 meets FDA requirements in 21 CFR 177.1520. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 3.0 g/10 min

@Temperature 230 °C
3.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F
Copyright © lookpolymers.com All Rights Reserved