A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Index of Compound 8.0 g/10 min

@Temperature 230 °C
8.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Gardner Impact 20.00 J

@Thickness 3.20 mm,
Temperature -30.0 °C
14.75 ft-lb

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648