Material Notes:
DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 8.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Strength 180 MPa
26100 psi
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Gardner Impact 10.8 J

@Temperature -30.0 °C
7.97 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Flame Spread <= 102 mm/min
<= 4.02 in/min