A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer A. Schulman, Inc.
Trade Name SCHULAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.012 cm/cm

@Thickness 3.175 mm
0.0030 - 0.012 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24600 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
Moisture Content 0.080 - 0.12 %
0.080 - 0.12 %