Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts, thixotropic additive.
Physical Properties Metric English Comments
Viscosity 15000 cP
15000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 6.0
6.0
Tensile Strength, Yield 2.00 MPa
290 psi
Elongation at Break 900 %
900 %
Tear Strength 14.0 kN/m
79.9 pli
Descriptive Properties Value Comments
Color White