Material Notes:
QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.Key Features: 90 minute room temperature cure One to one mix ratio 5 minute cure @ 150ºC Soft but resilient gel Designed for automatic mixing and dispensingPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
"B" component
0.970 g/cc
0.970 g/cc
"A" component
Viscosity 1000 cP
1000 cP
"B" component
1000 cP
1000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Penetration 5.0 - 9.0
5.0 - 9.0
mm, 30 mins @ 150°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Cure Time 5.000000 min

@Temperature 150 °C
0.08333334 hour

@Temperature 302 °F
10.00000 min

@Temperature 100 °C
0.1666667 hour

@Temperature 212 °F
90.0 min

@Temperature 25.0 °C
1.50 hour

@Temperature 77.0 °F
Gel Time 3.00 min
3.00 min
Descriptive Properties Value Comments
Color Transparent
"A" component
Transparent
"B" component