ACC QLE 1100 QSI Quantum Silicones 43 Durometer Clear, Addition Cure, 1-part Elastomer for Coating

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QLE 1100 QSI Quantum Silicones 43 Durometer Clear, Addition Cure, 1-part Elastomer for Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QLE 1100 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: 100% solids Transparent, ideal for pigmentation Fast cure at elevated temperatures Good abrasion resistance Primerless adhesion to many substrates Low viscosityPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
Viscosity 1000 cP
1000 cP
Storage Temperature <= 4.40 °C
<= 39.9 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
cured 30 mins @ 150°C
Tensile Strength, Yield 0.620 MPa
89.9 psi
cured 30 mins @ 150°C
Elongation at Break 50 %
50 %
cured 30 mins @ 150°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 200 °C
0.0833 hour

@Temperature 392 °F
30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color Clear/Light Brown