ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where low durometer, translucent material is requiredKey Features: Low viscosity High elongation Excellent retention of additional fluid Fast demold time Translucent and pigmentableMain Applications: Special Effects Skin replication Applications where pigmentation is requiredPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Uncatalyzed, QM CAT SKIN 30
1.12 g/cc
1.12 g/cc
Base
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT SKIN 30
30000 cP
30000 cP
catalyzed with QM CAT SKIN 30
50000 cP
50000 cP
Base
Linear Mold Shrinkage <= 0.0030 cm/cm
<= 0.0030 in/in
cured 72 hrs @ RT
Storage Temperature <= 38.0 °C
<= 100 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 5.0
5.0
cured 72 hrs @ RT
Tensile Strength, Yield 2.40 MPa
348 psi
cured 72 hrs @ RT
Elongation at Break 1000 %
1000 %
cured 72 hrs @ RT
Tear Strength 16.7 kN/m
95.0 pli
B, cured 72 hrs @ RT
Processing Properties Metric English Comments
Dry Time 16 - 24 hour
16 - 24 hour
Demold time, catalyzed with QM CAT SKIN 30
Cure Time 480 - 720 min
8.00 - 12.0 hour
Tack Free Time, catalyzed with QM CAT SKIN 30
Descriptive Properties Value Comments
Color Translucent
catalyzed with QM CAT SKIN 30
Translucent
Base
Translucent
Uncatalyzed, QM CAT SKIN 30
Work Life 42 mins
catalyzed with QM CAT SKIN 30