Material Notes:
AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a more cost-effective alternative for many applications now using AK Steel 18 Cr-Cb and Type 439 stainless steels. This alloy should also be considered for applications which Type 409 provides only marginal strength and oxidation resistance. ASTM Grain Size = 5 - 6.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.61 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 79 - 82

@Thickness 1.02 mm
79 - 82

@Thickness 0.0402 in
Tensile Strength, Ultimate 503 - 538 MPa

@Thickness 1.02 mm
73000 - 78000 psi

@Thickness 0.0402 in
Tensile Strength, Yield 345 - 372 MPa

@Strain 0.200 %,
Thickness 1.02 mm
50000 - 54000 psi

@Strain 0.200 %,
Thickness 0.0402 in
Elongation at Break 29 - 33 %
29 - 33 %
in 2 inches
Component Elements Properties Metric English Comments
Carbon, C 0.010 %
0.010 %
Chromium, Cr 11.35 %
11.35 %
Iron, Fe 86.325 %
86.325 %
As Remainder
Manganese, Mn 0.25 %
0.25 %
Nickel, Ni 0.20 %
0.20 %
Niobium, Nb (Columbium, Cb) 0.35 %
0.35 %
Nitrogen, N 0.015 %
0.015 %
Silicon, Si 1.3 %
1.3 %
Titanium, Ti 0.20 %
0.20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00007917 ohm-cm
0.00007917 ohm-cm