Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Precipitation Hardening Stainless
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, low-temperature heat treatments minimize distortion and scaling. AK Steel 15-5 PH® is the ferrite-free version of AK Steel 17-4 PH® Stainless Steel. Both alloys are widely used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries. The material supplied from the mill is in Condition A. After fabrication eight standard heat treatments have been developed to provide a wide range of properties.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 46
46
Longitudinal
46
46
Transverse
Tensile Strength, Ultimate 1438 MPa
208600 psi
Longitudinal
1466 MPa
212600 psi
Transverse
Tensile Strength, Yield 1385 MPa

@Strain 0.200 %
200900 psi

@Strain 0.200 %
Longitudinal
1393 MPa

@Strain 0.200 %
202000 psi

@Strain 0.200 %
Transverse
Elongation at Break 9.4 %
9.4 %
in 2 inches, Transverse
10.1 %
10.1 %
in 2 inches, Longitudinal
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 21.0 - 93.0 °C
6.00 µin/in-°F

@Temperature 69.8 - 199 °F
11.7 µm/m-°C

@Temperature <=427 °C
6.50 µin/in-°F

@Temperature <=801 °F
Thermal Conductivity 17.9 W/m-K

@Temperature 149 °C
124 BTU-in/hr-ft²-°F

@Temperature 300 °F
22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 14 - 15.5 %
14 - 15.5 %
Copper, Cu 2.5 - 4.5 %
2.5 - 4.5 %
Iron, Fe 71.91 - 79.85 %
71.91 - 79.85 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Nb + Ta 0.15 - 0.45 %
0.15 - 0.45 %
Nickel, Ni 3.5 - 5.5 %
3.5 - 5.5 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %