Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel 2205 Duplex Stainless steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 2205 Duplex Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 2205 provides a combination of high strength, excellent corrosion resistance and stress-corrosion cracking resistance as well as very good pitting resistance, and low thermal expansion. The alloy is useful in a variety of applications that include heat exchangers, piping, pressure vessels, tanks, fans, pulp and paper production equipment, oilfield equipment and press rolls.Information provided by AK Steel
Mechanical Properties Metric English Comments
Hardness, Rockwell C 22
22
Tensile Strength, Ultimate 750 MPa
109000 psi
Tensile Strength, Yield 510 MPa

@Strain 0.200 %
74000 psi

@Strain 0.200 %
Elongation at Break 35 %
35 %
in 2 inches
Charpy Impact, Notched 84.4 J/cm²

@Thickness 1.50 mm,
Temperature -40.0 °C
402 ft-lb/in²

@Thickness 0.0591 in,
Temperature -40.0 °F
Longitudinal
131 J/cm²

@Thickness 1.50 mm,
Temperature -40.0 °C
623 ft-lb/in²

@Thickness 0.0591 in,
Temperature -40.0 °F
Longitudinal
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 22 %
22 %
Iron, Fe 68.71 %
68.71 %
As Remainder
Molybdenum, Mo 3.1 %
3.1 %
Nickel, Ni 6.0 %
6.0 %
Nitrogen, N 0.17 %
0.17 %
Copyright © lookpolymers.com All Rights Reserved