AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Dent Resistant (DR 180)

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name ZINCGRIP® ELECTRASMOOTH®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Dent Resistant (DR 180).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compared to DS Type B, DR steels have higher initial YS which contributes to increased strength after forming.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 365 MPa
>= 52900 psi
Tensile Strength, Yield >= 214 MPa
>= 31000 psi
Elongation at Break >= 38 %
>= 38 %
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000142 ohm-cm
0.0000142 ohm-cm
Descriptive Properties Value Comments
Deep-Drawing Capability rm 1.7
Strain Hardening Exponent n 0.2