Material Notes:
AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig and fixture manufacturing, Tool manufacturing, Special machine construction, Standard parts. Information provided by ALIMEX GmbH
Physical Properties Metric English Comments
Density 2.829 g/cc
0.1022 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 145 - 180
145 - 180
Tensile Strength, Ultimate 460 - 590 MPa
66700 - 85600 psi
Rm
Tensile Strength, Yield 400 - 555 MPa

@Strain 0.200 %
58000 - 80500 psi

@Strain 0.200 %
Elongation at Break 4.0 - 11.5 %
4.0 - 11.5 %
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 165.01 W/m-K
1145.1 BTU-in/hr-ft²-°F
Descriptive Properties Value Comments
Machinability Good
Polishing Properties Good
Protective Anodizing Not decorative
Welding Properties (WIG, MIG) Suitable
Users viewing this material also viewed the following: