Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ALM TPE-210-S Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Elastomer, TPE
Manufacturer ALM Advanced Laser Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ALM TPE-210-S Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and abrasion resistance.TPE 210-S processes at a much lower temperature (~ 80 C) when compared to other commercially available flexible materials.TPE 210-S is 100% recyclableInformation provided by Advanced Laser Materials (ALM).
Physical Properties Metric English Comments
Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D1895
Density 1.03 g/cc
0.0372 lb/in³
Sintered; ASTM D792
Particle Size 20 - 130 µm
20 - 130 µm
D10-D90
85 µm
85 µm
D50
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 235 °C
16 g/10 min

@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 110 %
110 %
uninfiltrated; ASTM D638
Tensile Modulus 0.00800 GPa
1.16 ksi
ASTM D638
Flexural Modulus 0.00300 GPa

@Temperature 100 °C
0.435 ksi

@Temperature 212 °F
ASTM D790
0.0130 GPa

@Temperature 23.0 °C
1.89 ksi

@Temperature 73.4 °F
ASTM D790
0.0230 GPa

@Temperature -40.0 °C
3.34 ksi

@Temperature -40.0 °F
ASTM D790
Tear Strength 5.00 kN/m

@Temperature 100 °C
28.5 pli

@Temperature 212 °F
Initial, Die C; ASTM D624
6.00 kN/m

@Temperature 23.0 °C
34.2 pli

@Temperature 73.4 °F
Initial, Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 353
353
H-18 Wheel; ASTM D4060
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
ASTM D3418
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+13 ohm-cm
1.50e+13 ohm-cm
ASTM D257
Surface Resistance 1.90e+13 ohm
1.90e+13 ohm
ASTM D257
Dielectric Constant 2.9
2.9
Descriptive Properties Value Comments
Shore Hardness (scale not noted) 40
uninfiltrated, ASTM D2240
Copyright © lookpolymers.com All Rights Reserved